Mechanical Properties Metric English Comments
Tensile Strength, Yield 14.0 - 35.0 MPa
2030 - 5080 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 31008 PVDF Copolymer  (discontinued **)
Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General ..
Tensile Strength, Yield 14.0 - 35.0 MPa
2030 - 5080 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 32008 PVDF Copolymer  (Unverified Data**)
Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General ..
Tensile Strength, Yield 8.80 - 35.0 MPa
1280 - 5080 psi
Average value: 19.4 MPa Grade Count:34
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..
Tensile Strength, Yield 20.0 - 35.0 MPa

@Thickness 2.00 mm
2900 - 5080 psi

@Thickness 0.0787 in
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)
Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Features: Copolymer; Good Flexibility; Medium ViscosityAdditional Properties: Crystal..
Tensile Strength, Yield 14.0 - 35.0 MPa

@Thickness 2.00 mm
2030 - 5080 psi

@Thickness 0.0787 in
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
Tensile Strength, Yield 14.0 - 35.0 MPa

@Thickness 2.00 mm
2030 - 5080 psi

@Thickness 0.0787 in
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF)
Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
Tensile Strength, Yield 22.0 - 35.0 MPa
3190 - 5080 psi
Spec; ISO 527-1/2
Axion Polymers Axpoly® PP06 5001 Enhanced Black General Purpose Polypropylene
PP06 Series polypropylene offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PP06 range of resin co..
Tensile Strength, Yield 20.0 - 35.0 MPa

@Thickness 2.00 mm,
Temperature 23.0 °C
2900 - 5080 psi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type IV, 50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Tensile Strength, Yield 14.0 - 35.0 MPa

@Thickness 2.00 mm,
Temperature 23.0 °C
2030 - 5080 psi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type IV, 50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers.
Tensile Strength, Yield 30.0 - 35.0 MPa
4350 - 5080 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer  (discontinued **)
Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD..
Tensile Strength, Yield 1.18 - 35.0 MPa
171 - 5080 psi
Average value: 13.1 MPa Grade Count:65
Overview of materials for Polyether Ester Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr..