Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axion Polymers Axpoly® PP06 5001 Enhanced Black General Purpose Polypropylene

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Axion Polymers
Trade Name Axpoly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axion Polymers Axpoly® PP06 5001 Enhanced Black General Purpose Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PP06 Series polypropylene offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PP06 range of resin compounds are processed to a high purity and give consistent material properties during injection molding and sheet extrusion.Produced from 100% post-consumer raw materials, this product fits closely with Axion's other recycled resin grades and offers the same set of user benefits, including:Successfully replaces virgin resinHuge savings in CO2 impactAppeals to 'greener' customersCost-down on raw materialInformation provided by Axion Recycling
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
Typical; ISO 1183-1
0.922 - 1.00 g/cc
0.0333 - 0.0361 lb/in³
Spec; ISO 1183-1
Particle Size 2000 - 4000 µm
2000 - 4000 µm
Pellet Size
3000 µm
3000 µm
Typical
Melt Index of Compound 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Typical
9.0 - 16 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 - 16 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Spec
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
Typical; ISO 527-1/2
22.0 - 35.0 MPa
3190 - 5080 psi
Spec; ISO 527-1/2
Izod Impact, Unnotched (ISO) 7.00 - 11.0 kJ/m²
3.33 - 5.23 ft-lb/in²
Spec; ISO 180
9.00 kJ/m²
4.28 ft-lb/in²
Typical; ISO 180
Processing Properties Metric English Comments
Moisture Content 0.17 %
0.17 %
Typical
<= 0.25 %
<= 0.25 %