Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Statiblend® 02020 MB Polypropylene, 5% Glass Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Glass Fiber Filler
Manufacturer Techmer ES
Trade Name Statiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Statiblend® 02020 MB Polypropylene, 5% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 5% Filler by Weight/Unspecified FillerReinforFeatures: ConductiveTPCI# 9117116Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0080 cm/cm

@Thickness 3.17 mm
0.0080 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 4.0 g/10 min

@Load 10.0 kg,
Temperature 230 °C
4.0 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Strength 29.0 MPa
4200 psi
ASTM D790
Flexural Modulus 1.65 GPa
240 ksi
ASTM D790
Izod Impact, Notched 2.14 J/cm

@Thickness 3.17 mm
4.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.3 °C
200 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity <= 1000 ohm-cm
<= 1000 ohm-cm
ASTM D257
Surface Resistance <= 1.00e+6 ohm
<= 1.00e+6 ohm
ASTM D257
Static Decay <= 2.0 sec
<= 2.0 sec
MIL B-81705C