Clariant OMAN698583 Thermoplastic Polyurethane, Halogen Free, Flame Retardant

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Clariant
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant OMAN698583 Thermoplastic Polyurethane, Halogen Free, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aromatic Polyether BasedData provided by Clariant Masterbatches
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
ASTM D2240
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D412
5.17 MPa

@Strain 100 %
750 psi

@Strain 100 %
ASTM D412
8.96 MPa

@Strain 300 %
1300 psi

@Strain 300 %
ASTM D412
Elongation at Break 620 %
620 %
ASTM D412
Tear Strength 59.6 kN/m
340 pli
Die C; ASTM D624
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
Processing Properties Metric English Comments
Rear Barrel Temperature 182 - 193 °C
360 - 380 °F
Middle Barrel Temperature 188 - 193 °C
370 - 380 °F
Front Barrel Temperature 188 - 193 °C
370 - 380 °F
Melt Temperature 188 - 196 °C
370 - 385 °F