Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PPC 5724 Polypropylene, Extra High Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Total Atofina
Trade Name PPC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPC 5724 Polypropylene, Extra High Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ATOFINA 5724 is characterized by a high fluidity offering a combination of processing and excellent impact properties in applications ranging from industrial to household.ApplicationATOFINA 5724 has been developed with improved gloss and excellent color for the manufacture of garden furniture, automotive applications, caps, closures, paint containers and toys requiring extra toughness. Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 0.896 GPa
130 ksi
ASTM D 790
Izod Impact, Notched 0.750 J/cm
1.41 ft-lb/in
Low Temp; ASTM D256
NB
NB
ASTM D256
Thermal Properties Metric English Comments
Melting Point 160 - 165 °C
320 - 329 °F
ATOFINA Method
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C
187 °F
ASTM D648
Vicat Softening Point 143 °C
289 °F
ASTM D1525