Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Delrin® 111DP NC010 Acetal (POM)  (Unverified Data**)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced
Manufacturer DuPont Performance Polymers
Trade Name Delrin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Delrin® 111DP NC010 Acetal (POM)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nucleated High Viscosity Acetal Homopolymer Delrin 111DP is a new high viscosity acetal homopolymer with enhanced crystallization and excellent creep and fatigue resistance. It has improved thermal stability excellent dimensional stability low warpageInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
1.42 g/cc
0.0513 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.020 cm/cm
0.020 in/in
ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.019 cm/cm
0.019 in/in
ISO 294-4 2577
Melt Flow 2.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 72.0 MPa
10400 psi
ISO 527-1/-2
Elongation at Break 40 %
40 %
Nominal; ISO 527-1/-2
Elongation at Yield 20 %
20 %
ISO 527-1/-2
Tensile Modulus 3.15 GPa
457 ksi
ISO 527-1/-2
Flexural Modulus 2.95 GPa
428 ksi
ISO 178
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
ISO 179/1eA
1.00 J/cm²

@Temperature -40.0 °C
4.76 ft-lb/in²

@Temperature -40.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Specific Heat Capacity 3.00 J/g-°C
0.717 BTU/lb-°F
Thermal Conductivity 0.220 W/m-K
1.53 BTU-in/hr-ft²-°F
of melt
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 165 °C
329 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C
208 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
IEC 60695-11-10
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
IEC 60695-11-10
Descriptive Properties Value Comments
Additives Lubricants
Release agent
Delivery Form Pellets
Part Marking Code >POM<
ISO 11469
Processing Injection Moulding
Other Extrusion
Profile Extrusion
Sheet Extrusion
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification POM
ISO 1043
UL recognition UL