Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 71.6 MPa @Thickness 3.20 mm |
10400 psi @Thickness 0.126 in |
ASTM D638 |
LG Chemical LUMILOY GN1306F Injection Molding FR Heat Resistant mPPO Uses include electric/electronic parts. |