Polymer Property : Izod Impact, Notched (ISO) = 0.904 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 1.90 - 14.0 kJ/m²

@Temperature -40.0 - -30.0 °C
0.904 - 6.66 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 5.84 kJ/m² Grade Count:3
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
Izod Impact, Notched (ISO) 1.90 kJ/m²
0.904 ft-lb/in²
ISO 180/1A
Lucite International Diakon® CLH952 Acrylic Polymer
Information provided by Lucite International
Izod Impact, Notched (ISO) 1.90 kJ/m²
0.904 ft-lb/in²
ISO 180/1A
Lucite International Diakon® CLH952L Acrylic Polymer
Information provided by Lucite International
Izod Impact, Notched (ISO) 1.90 kJ/m²
0.904 ft-lb/in²
ISO 180/1A
Lucite International Diakon® CLH952LX Acrylic Polymer
Information provided by Lucite International
Izod Impact, Notched (ISO) 1.90 - 1.90 kJ/m²

@Temperature -40.0 - -40.0 °C
0.904 - 0.904 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 1.90 kJ/m² Grade Count:1
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..