Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 1.90 - 14.0 kJ/m² @Temperature -40.0 - -30.0 °C |
0.904 - 6.66 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 5.84 kJ/m² Grade Count:3 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Izod Impact, Notched (ISO) | 1.90 kJ/m² | 0.904 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® CLH952 Acrylic Polymer Information provided by Lucite International |
|||
Izod Impact, Notched (ISO) | 1.90 kJ/m² | 0.904 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® CLH952L Acrylic Polymer Information provided by Lucite International |
|||
Izod Impact, Notched (ISO) | 1.90 kJ/m² | 0.904 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® CLH952LX Acrylic Polymer Information provided by Lucite International |
|||
Izod Impact, Notched (ISO) | 1.90 - 1.90 kJ/m² @Temperature -40.0 - -40.0 °C |
0.904 - 0.904 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 1.90 kJ/m² Grade Count:1 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |