Material Notes:
Description: TECHNYL® C 216 V40 is a polyamide 6, reinforced with 40% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers a good combination between thermal and mechanical properties.Available in: Europe and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: It is used in a wide variety of industries.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 140 MPa
20300 psi
ISO 527 Type 1A
Elongation at Break 3.5 %
3.5 %
ISO 527 Type 1A
Tensile Modulus 7.30 GPa
1060 ksi
ISO 527 Type 1A
Flexural Modulus 7.20 GPa
1040 ksi
ISO 178
Izod Impact, Notched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 11.5 J/cm²
54.7 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 3.40 J/cm²
16.2 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 22.0 kV/mm
559 kV/in
IEC 60243
Dissipation Factor 0.090
0.090
IEC 60250
Comparative Tracking Index 475 V
475 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %