BASF Ultradur® B 4040 G2 10% Glass Filled PBT + PET

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + PET Blend, Glass Filled , Polyethylene Terephthalate (PET)
Manufacturer BASF
Trade Name Ultradur®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultradur® B 4040 G2 10% Glass Filled PBT + PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Is a PBT + PET, injection-molding grade containing 10% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housings for vehicles, headlamp frames, cams, automotive windscreen wiper arms, PCBs, housings, consoles, contact mounts and covers.Information provided by BASF
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
Water Absorption 0.40 %
0.40 %
Saturation; DIN 53495/1L
Moisture Absorption at Equilibrium 0.20 %
0.20 %
23°C; 50% RH
Viscosity Measurement 107
107
[ml/g]; Viscosity number; ISO 1628
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
Sheet
Linear Mold Shrinkage, Transverse 0.012 cm/cm
0.012 in/in
Sheet
Melt Flow 33.36 g/10 min

@Load 2.16 kg,
Temperature 275 °C
33.36 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 96.0 MPa
13900 psi
50 mm/min; ISO 527-2
Elongation at Yield 2.9 %
2.9 %
50 mm/min; ISO 527-2
Modulus of Elasticity 5.00 GPa
725 ksi
ISO 527-2
Charpy Impact Unnotched 2.60 J/cm²
12.4 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.380 J/cm²
1.81 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 - 250 °C
428 - 482 °F
DSC; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
421 °F
ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 168 °C
334 °F
ISO 75-2
Processing Properties Metric English Comments
Melt Temperature 250 - 275 °C
482 - 527 °F
Injection-molding
270 °C
518 °F
for shrinkage test
Mold Temperature 60.0 - 100 °C
140 - 212 °F
80.0 °C
176 °F
for shrinkage test
Descriptive Properties Value Comments
Color Colored and Black
Commercial Status Europe
Primary Processing Technique Injection Molding