DSM Arnite® B600SE PBT FR

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Flame Retardant
Manufacturer DSM Engineering Plastics
Trade Name Arnite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Arnite® B600SE PBT FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame Retardant
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 60.0 MPa
8700 psi
ISO 527-1/-2
Elongation at Break 4.0 %
4.0 %
ISO 527-1/-2
Tensile Modulus 3.00 GPa
435 ksi
ISO 527-1/-2
Charpy Impact Unnotched 2.40 J/cm²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
IEC 60695-11-10