Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.392 - 4.00 J/cm | 0.735 - 7.49 ft-lb/in | Average value: 1.77 J/cm Grade Count:104 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Izod Impact, Notched | 0.480 - 4.00 J/cm @Temperature -40.0 - 0.000 °C |
0.899 - 7.49 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 1.28 J/cm Grade Count:13 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched | 0.480 - 4.00 J/cm @Thickness 3.17 - 6.40 mm |
0.899 - 7.49 ft-lb/in @Thickness 0.125 - 0.252 in |
Average value: 1.28 J/cm Grade Count:13 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched | 0.167 - 4.00 J/cm | 0.312 - 7.49 ft-lb/in | Average value: 1.63 J/cm Grade Count:17 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Izod Impact, Notched | 3.00 - 4.00 J/cm @Temperature 23.0 °C |
5.62 - 7.49 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Loxim 500 00HB Polycarbonate/Acrylonitrile Butadiene Styrene Information provided by Loxim Industries |
|||
Izod Impact, Notched | 2.00 - 4.00 J/cm @Temperature -40.0 - -20.0 °C |
3.75 - 7.49 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 3.00 J/cm Grade Count:1 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |