Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loxim 500 00HB Polycarbonate/Acrylonitrile Butadiene Styrene

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Loxim Industries
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loxim 500 00HB Polycarbonate/Acrylonitrile Butadiene Styrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.12 - 1.15 g/cc
1.12 - 1.15 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 - 55.0 MPa
7250 - 7980 psi
ASTM D683
Flexural Strength 80.0 - 90.0 MPa
11600 - 13100 psi
ASTM D790
Flexural Modulus 2.40 - 2.80 GPa
348 - 406 ksi
ASTM D790
Izod Impact, Notched 3.00 - 4.00 J/cm

@Temperature 23.0 °C
5.62 - 7.49 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 - 120 °C
230 - 248 °F
ASTM D1525, HDT Method B
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Users viewing this material also viewed the following: