Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.167 - 4.00 J/cm | 0.312 - 7.49 ft-lb/in | Average value: 1.63 J/cm Grade Count:17 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Izod Impact, Notched | 0.167 J/cm | 0.313 ft-lb/in | ASTM D256 |
Plenco 05118-T5 Phenolic, Granular, Compression Molded PLENCO 05118-T5 is a mineral and graphite filled novolac phenolic molding compound with PTFE, formulated for bearing seals. 05118 provides for a low coefficient of friction, good wear resistance, ve.. |
|||
Izod Impact, Notched | 0.167 J/cm | 0.312 ft-lb/in | ASTM D256 |
E-Polymers SEPAZ® C230GP 30% Glass Fiber Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |