Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical SEETEC M1315 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer LG Chemical
Trade Name SEETEC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical SEETEC M1315 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: SEETEC M1315 is a heterophasic polypropylene copolymer for compression molding caps, especially SACMI machines. SEETEC M1315 exhibits an excellent stiffness, a high impact strength, a high productivity and a good processability. SEETEC M1315 meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520 for food contact.Applications: Bottle Caps and ClosuresCAS No. 9010-79-1Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D1505
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 30.4 MPa
4410 psi
50mm/min; ASTM D638
Flexural Modulus 1.72 GPa
249 ksi
ASTM D760
Izod Impact, Notched 0.785 J/cm

@Temperature 23.0 °C
1.47 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 130 - 170 °C
266 - 338 °F
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648
Vicat Softening Point 154 °C

@Load 1.00 kg
309 °F

@Load 2.20 lb
ASTM D1525
Flash Point >= 340 °C
>= 644 °F
Descriptive Properties Value Comments
Autoignition Temperature >350°C
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved