Kolon KOPET® KP133G45 FR-PET Resin

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 50% Glass Reinforced
Manufacturer Kolon
Trade Name KOPET®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon KOPET® KP133G45 FR-PET Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of product, good harmonized mechanical properties with flame retardInformation provided by US distributor, API-Kolon.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
DIN 53479; ASTM D792
Water Absorption 0.050 %
0.050 %
DIN 53475; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
DIN 53505; ASTM D785
Tensile Strength, Ultimate 142 MPa
20600 psi
DIN 53455; ASTM D638
Elongation at Break 4.0 %
4.0 %
DIN 53455; ASTM D638
Flexural Yield Strength 235 MPa
34100 psi
DIN 53455; ASTM D790
Flexural Modulus 9.81 GPa
1420 ksi
DIN 53452; ASTM D790
Izod Impact, Notched 0.785 J/cm
1.47 ft-lb/in
DIN 53453; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 25.0 µm/m-°C

@Temperature 20.0 °C
13.9 µin/in-°F

@Temperature 68.0 °F
DIN 53752; ASTM D696
Melting Point 254 °C
489 °F
DIN 53736; ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 226 °C
439 °F
DIN 53461; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.9

@Frequency 1e+6 Hz
3.9

@Frequency 1e+6 Hz
ASTM D150/DIN 53483
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149/DIN 53481
Arc Resistance 120 sec
120 sec
ASTM D495
Users viewing this material also viewed the following: