Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.400 - 0.500 J/cm | 0.749 - 0.937 ft-lb/in | ASTM D256-06 |
Proto3000 Objet DurusWhite FullCure430 Polypropylene-like Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Izod Impact, Notched | 0.400 - 0.500 J/cm @Temperature -40.0 - -20.0 °C |
0.749 - 0.937 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.168 J/cm Grade Count:1 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.500 - 0.500 J/cm @Temperature -29.0 - -29.0 °C |
0.937 - 0.937 ft-lb/in @Temperature -20.2 - -20.2 °F |
Average value: 0.500 J/cm Grade Count:1 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.300 - 0.500 J/cm @Temperature -30.0 - 0.000 °C |
0.562 - 0.937 ft-lb/in @Temperature -22.0 - 32.0 °F |
Average value: 0.579 J/cm Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Izod Impact, Notched | 0.300 - 0.500 J/cm @Thickness 3.20 - 3.20 mm |
0.562 - 0.937 ft-lb/in @Thickness 0.126 - 0.126 in |
Average value: 0.579 J/cm Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Izod Impact, Notched | 0.400 - 0.500 J/cm @Temperature -30.0 - 0.000 °C |
0.749 - 0.937 ft-lb/in @Temperature -22.0 - 32.0 °F |
Average value: 0.475 J/cm Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Izod Impact, Notched | 0.400 - 0.500 J/cm @Thickness 3.20 - 3.20 mm |
0.749 - 0.937 ft-lb/in @Thickness 0.126 - 0.126 in |
Average value: 0.475 J/cm Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Izod Impact, Notched | 0.450 - 0.500 J/cm @Temperature -30.0 - 0.000 °C |
0.843 - 0.937 ft-lb/in @Temperature -22.0 - 32.0 °F |
Average value: 0.475 J/cm Grade Count:1 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched | 0.500 - 0.500 J/cm @Temperature -40.0 - -40.0 °C |
0.937 - 0.937 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.500 J/cm Grade Count:1 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Izod Impact, Notched | 0.450 - 0.500 J/cm | 0.843 - 0.937 ft-lb/in | ASTM D256 |
Loxim 330 12V0 Nylon 6 Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.400 - 0.500 J/cm | 0.749 - 0.937 ft-lb/in | ASTM D256 |
Loxim 820 12 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.400 - 0.500 J/cm | 0.749 - 0.937 ft-lb/in | ASTM D256 |
Loxim 810 01 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.400 - 0.500 J/cm | 0.749 - 0.937 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Izod Impact, Notched | 0.400 - 0.500 J/cm | 0.749 - 0.937 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 135 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics: Self lubricating Good mechanical strength Low co-efficient of friction Good thermal conductivity Heat stable (200°C) Good mouldability Not suitable for electrical application Color.. |
|||
Izod Impact, Notched | 0.400 - 0.500 J/cm | 0.749 - 0.937 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATO 159 Phenolic Molding Glass/ inorganic Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Izod Impact, Notched | 0.210 - 0.500 J/cm @Temperature -40.0 - -40.0 °C |
0.393 - 0.937 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.374 J/cm Grade Count:11 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Notched | 0.200 - 0.500 J/cm @Temperature -18.0 - -18.0 °C |
0.375 - 0.937 ft-lb/in @Temperature -0.400 - -0.400 °F |
Average value: 0.325 J/cm Grade Count:4 |
Overview of materials for Acrylic, Impact Modified Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.200 - 0.500 J/cm @Temperature -18.0 - -18.0 °C |
0.375 - 0.937 ft-lb/in @Temperature -0.400 - -0.400 °F |
Average value: 0.275 J/cm Grade Count:4 |
Overview of materials for Acrylic, Optical Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr.. |