Loxim 810 01 HB Polypropylene Compound, Flame Retardant

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer Loxim Industries
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loxim 810 01 HB Polypropylene Compound, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 0.920 - 1.02 g/cc
0.920 - 1.02 g/cc
ASTM D792
Filler Content 10 %
10 %
Linear Mold Shrinkage 0.0090 - 0.011 cm/cm
0.0090 - 0.011 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.0 - 39.0 MPa
5370 - 5660 psi
ASTM D683
Elongation at Break 14 - 16 %
14 - 16 %
ASTM D638
Flexural Modulus 2.00 - 2.50 GPa
290 - 363 ksi
ASTM D790
Izod Impact, Notched 0.400 - 0.500 J/cm
0.749 - 0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 - 110 °C
212 - 230 °F
ASTM D1525, HDT Method B
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in