Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Amity Thermosets ATS 135 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic
Manufacturer Amity Thermosets
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amity Thermosets ATS 135 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: Self lubricating Good mechanical strength Low co-efficient of friction Good thermal conductivity Heat stable (200°C) Good mouldability Not suitable for electrical application Color-blackMedium flow Applications:Grinding disc centres CastorsGas meter partsGas regulator knobs, etc. Information provided by Amity Thermosets Limited
Physical Properties Metric English Comments
Density 1.60 - 1.75 g/cc
0.0578 - 0.0632 lb/in³
Molding; IS 867-1963
Apparent Bulk Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
IS 867-1963
Water Absorption 0.15 - 0.25 %
0.15 - 0.25 %
IS 13411-1993
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
IS 13411-1992
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 - 60.0 MPa
7250 - 8700 psi
5 mm/min.; IS 867-1963
Shear Strength 80.0 - 90.0 MPa
11600 - 13100 psi
IS 867-1963
Izod Impact, Notched 0.400 - 0.500 J/cm
0.749 - 0.937 ft-lb/in
IS 13411-1992
Processing Properties Metric English Comments
Mold Temperature 160 - 180 °C
320 - 356 °F
Injection Pressure 15.68 - 34.3 MPa
2274 - 4970 psi
Mold Pressure
Cure Time 1.08 - 1.33 min
0.0181 - 0.0222 hour
per mm
Shelf Life 12.0 Month
12.0 Month
10-25°C