Material Notes:
Homopolymer for injection molding. Meets General Motors spec. GMP.PP.013Data provided by Washington Penn Plastic Co., Inc.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Melt Flow 6.0 g/10 min
6.0 g/10 min
Cond L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa
4640 psi
ASTM D638
Flexural Modulus 1.40 GPa
203 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.300 J/cm

@Thickness 3.17 mm
0.562 ft-lb/in

@Thickness 0.125 in
ASTM D256
Gardner Impact 2.30 J
1.70 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM D648