Polyram PlusTek PB901 Nylon 6, Extruded cable coating

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Extruded
Manufacturer Polyram
Trade Name PlusTek
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PB901 Nylon 6, Extruded cable coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyamide 6 for very thin electrical extruded cable coatingInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
DIN 53479
Water Absorption 1.9 %
1.9 %
DIN 53495
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 85.0 MPa
12300 psi
ASTM-D638
Elongation at Break 100 %
100 %
ASTM-D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 2.50 GPa
363 ksi
ASTM-D790
Izod Impact, Notched 0.300 J/cm

@Temperature 23.0 °C
0.562 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous Use
150 °C
302 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
DIN 53461
Flammability, UL94 V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
DIN 53482
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
DIN 53482
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 100 kV/mm
2540 kV/in
VDE 0303/4