Polymer Property : Charpy Impact, Notched = 0.952 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.140 - 0.200 J/cm²
0.666 - 0.952 ft-lb/in²
Compression; ISO 179/1eA
Raschig Group MELOPAS® 2010 MF Melamine
Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav..
Charpy Impact, Notched 0.150 - 0.200 J/cm²
0.714 - 0.952 ft-lb/in²
Injection; ISO 179/1eA
Raschig Group MELOPAS® 2010 MF Melamine
Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav..
Charpy Impact, Notched 0.130 - 0.200 J/cm²
0.619 - 0.952 ft-lb/in²
Injection; ISO 179/1eA
Raschig Group MELOPAS® 6605 MP Melamine
Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be..
Charpy Impact, Notched 0.100 - 0.200 J/cm²
0.476 - 0.952 ft-lb/in²
Compression; ISO 179/1eA
Raschig Group RALUPOL® 2100 UP Polyester
Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta..
Charpy Impact, Notched 0.200 - 0.200 J/cm²

@Temperature -30.0 - -20.0 °C
0.952 - 0.952 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.200 J/cm² Grade Count:4
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
Charpy Impact, Notched 0.100 - 0.200 J/cm²
0.476 - 0.952 ft-lb/in²
ISO 179
Vyncolit 3640 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..
Charpy Impact, Notched 0.200 - 0.200 J/cm²

@Temperature -20.0 - -20.0 °C
0.952 - 0.952 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.200 J/cm² Grade Count:1
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..