Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB SCANFILL Injection CPC35051 PP/PE, Mineral Reinforced

Category Polymer , Thermoplastic , Polyethylene (PE) , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Polykemi AB
Trade Name SCANFILL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB SCANFILL Injection CPC35051 PP/PE, Mineral Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Filler Content 51 %
51 %
±2%; Polykemi
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
With Flow; ISO 2577
0.011 cm/cm
0.011 in/in
Across Flow; ISO 2577
Melt Index of Compound 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Elongation at Yield 2.0 %
2.0 %
ISO/R527
Flexural Strength <= 35.0 MPa
<= 5080 psi
ISO 178
Flexural Modulus 3.50 GPa

@Temperature 23.0 °C
508 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
120°C/h; ISO 75/1
Vicat Softening Point 86.0 °C

@Load 5.001 kg
187 °F

@Load 11.03 lb
50°C/h; ISO 306
151 °C

@Load 1.00 kg
304 °F

@Load 2.21 lb
50°C/h; ISO 306