Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 2311 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Woodflour Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 2311 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide improved pourability characteristics for cold powder compression molding. UL recognized under component file E40654. 02311 is available in black or brown color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.580 g/cc
0.0210 lb/in³
ASTM D1895
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Water Absorption 0.53 %
0.53 %
ASTM D570
Linear Mold Shrinkage 0.0034 cm/cm
0.0034 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 88
88
ASTM D785
Tensile Strength, Ultimate 55.0 MPa
7980 psi
ASTM D638
Elongation at Break 0.63 %
0.63 %
ASTM D638
Tensile Modulus 9.40 GPa
1360 ksi
ASTM D638
Flexural Strength 92.0 MPa
13300 psi
ASTM D790
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Compressive Strength 209 MPa
30300 psi
ASTM D695
Izod Impact, Notched 0.207 J/cm
0.388 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ASTM D256
Impact 137
137
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 67.0 µm/m-°C

@Temperature 40.0 - 130 °C
37.2 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.410 W/m-K

@Temperature 100 °C
2.85 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 196 °C
385 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 176 °C
349 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 26 %
26 %
ASTM D2863
Shrinkage 0.233 %
0.233 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.30e+12 ohm-cm
2.30e+12 ohm-cm
ASTM D247
Dielectric Constant 5.1
5.1
ASTM D150
Dielectric Strength 14.1 kV/mm
358 kV/in
Short Time; ASTM D149
Dissipation Factor 0.045
0.045
ASTM D150
Arc Resistance 135 sec
135 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638
Users viewing this material also viewed the following: