Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco Valite 4100 Novolac Phenolic, Granular, Compression Molded  (discontinued **)

Category Polymer , Thermoset , Phenolic
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco Valite 4100 Novolac Phenolic, Granular, Compression Molded  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This Valite product has been replaced by Plenco 4100. Data provided by Plenco.VALITE 4100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in applicance and oil field applications and can be molded by compression, transfer, or injection processes. It is UL recognized under component file E59891. VALITE 4100 is the same formulation as PLENCO 04100. Plenco drop ball 113g test value is 28 cm.Plenco has discontinued their Valite product line.
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Apparent Bulk Density 0.730 g/cc
0.0264 lb/in³
ASTM D1895
Water Absorption 0.25 %
0.25 %
ASTM D570
Linear Mold Shrinkage 0.0037 cm/cm
0.0037 in/in
Post shrinkage is 0.12% at 72hr 120°C.; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 86
86
ASTM D785
Tensile Strength, Ultimate 60.9 MPa
8830 psi
ASTM D638
Elongation at Break 0.70 %
0.70 %
ASTM D638
Tensile Modulus 10.6 GPa
1540 ksi
ASTM D638
Flexural Yield Strength 80.0 MPa
11600 psi
ASTM D790
Flexural Modulus 9.50 GPa
1380 ksi
ASTM D790
Compressive Yield Strength 207.9 MPa
30150 psi
ASTM D695
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
J/cm; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Heat Resistance; ASTM D795
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.47 mm
V-1

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 3.40e+12 ohm-cm
3.40e+12 ohm-cm
ASTM D257
Dielectric Constant 4.8

@Frequency 1e+6 Hz
4.8

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 15.1 kV/mm
384 kV/in
Short Term per ASTM D149.
Dissipation Factor 0.038

@Frequency 1e+6 Hz
0.038

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 160 sec
160 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638
Copyright © lookpolymers.com All Rights Reserved