Mechanical Properties Metric English Comments
Ball Indentation Hardness 20.0 - 230 MPa
2900 - 33400 psi
Average value: 122 MPa Grade Count:59
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Ball Indentation Hardness 20.0 MPa
2900 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® XE 3982 PA12
Product description: Grilamid XE 3982 is a highly flexible extrusion grade, based on Polyamide 12 with following main attributes: High flexibilityLow plasticizer migration (low blooming)Very good ch..