Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 155 MPa | 22500 psi | ISO2039.1 DIN.53456 |
Omnia Plastica Omniamid PA 6 - Akulon 6 - Dry Semi-crystalline polymer of polyamide obtained by the polymerisation of the caprolactam. Its large popularity is due to both its good overall features as well as its cost-performance relationship. T.. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | ISO 2039-1 |
Polycasa XT 630 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | ISO 2039-1 |
Nilit FRIANYL A63 HH-GV40 Nylon 6.6 for injection molding, 40% glass fiber reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | ISO 2039-1 |
Nilit FRIANYL A63 SG40 Nylon 6.6 for injection molding, 40% mineral filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | ISO 2039-1 |
Quadrant EPP Acetron® MD POM-C + metal detectable additive, extruded (ISO Data) Metal detectable POM-C grade High mechanical strength, stiffness and hardness Excellent resilience Good creep resistance High impact strength, even at low temperatures Very good dimensional stabilit.. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | ISO 2039-1 |
Nilit FRIANYL C73 H-GV15 Nylon 6.6/6 for injection molding, 15% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | ISO 2039-1 |
Nilit FRIANYL A63 CV-CU 0550 Nylon 6.6 for injection molding, 5% carbon fiber reinforced, 50% copper filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | ISO 2039-1 |
Nilit FRIANYL B63 GV10 Nylon 6 for injection molding, 10% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | ISO 2039-1 |
Nilit FRIANYL B63 GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | ISO 2039-1 |
Nilit FRIANYL B63 H-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 155 - 230 MPa | 22500 - 33400 psi | Average value: 189 MPa Grade Count:16 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | ISO 2039-1 |
Lanxess Durethan® DP BKV 30 XF 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LBV-30H FWA black 9225 PA12-GF30 Product Description: Grilamid LBV-30H FWA black 9225 is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined wit.. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LV-50H FWA black 9225 PA12-GF50 Product description: Grilamid LV-50H FWA black 9225 is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LV-50H FWA nat PA12-GF50 Product description: Grilamid LV-50H FWA natural is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 3915 PA12-GF50 Product description: Grilamid XE 3915 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following produce profile:Good UV StabilityHigh impact strengthVe.. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4104 black 9992 PA610-GF40 Product description: Grilamid XE 4104 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4107 black 9992 PA612-GF40 Product description: Grilamid XE 4107 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorpti.. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4107 nat PA612-GF40 Product description: Grilamid XE 4107 natural is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorptiong.. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | H358/30; ISO 2039-1 |
Chi Mei Kibisan® PN-106 L150 SAN High Clarity |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | H358/30; ISO 2039-1 |
Chi Mei Kibisan® PN-107 L125 SAN High Clarity |
|||
Ball Indentation Hardness | 155 MPa @Time 30.0 sec |
22500 psi @Time 0.00833 hour |
DIN 53 456 |
Hippe POM Copolymer Polyacetals are particularly suitable for the manufacture of precision and technical components, bushing, spring elements, housing components, sliding elements, chains, curve discs, bearing, running.. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BG-50 H PA6-GF50 Product description: Grilon BG-50 H is a high heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 H has the following important properties: High stiffnessHigh heat resist.. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BG-50 S PA6-GF50 Product description: Grilon BG-50 S is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 S has the following important properties: High stiffnessExcellent surface fin.. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LBV-30H FWA nat PA12-GF30 Product Description: Grilamid LBV-30H FWA natural is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h.. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 411 POM Easy flowing, internally strengthened grade for injection molding of thin walled parts of very high mechanical requirements.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTRO HPM Polysulfone This plastic has good hydrolysis, chemical and radiation resistance, and can operate at high temperatures. It is used in food processing industry, pumps and valves, and medical equipment.Informatio.. |
|||
Ball Indentation Hardness | 155 MPa | 22500 psi | ISO 2039 |
BASF Ultraform S 1320 0021 UNC POM Ultraform S1320 0021 UNC is an easy flowing, rapidly freezing injection molding POM grade with enhanced stiffness and heat distortion resistance. It is highly stabilized to resist aggressive fuels,.. |