Mechanical Properties Metric English Comments
Compressive Yield Strength 152 MPa
22000 psi
ASTM D695
Plenco 50015 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 50015 is an engineering grade glass reinforced polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL recognized and available in white, natu..
Compressive Yield Strength 152 MPa
22000 psi
Average value: 152 MPa Grade Count:3
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Ea..
Compressive Yield Strength 152 - 434 MPa
22000 - 62900 psi
Average value: 199 MPa Grade Count:32
Overview of materials for Phenolic, Novolac, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values..
Compressive Yield Strength 152 - 172 MPa
22000 - 25000 psi
Average value: 164 MPa Grade Count:4
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Compressive Yield Strength 152 MPa
22000 psi
ASTM D695
Sumitomo Bakelite North America 3-2-530 Short-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A..
Compressive Yield Strength 152 MPa
22000 psi
ASTM D695
Sumitomo Bakelite North America RX® 3-1-525F-P Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I..
Compressive Yield Strength 152 MPa
22000 psi
ASTM D695
Sumitomo Bakelite North America RX® 3-2-520F-P Short-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI..
Compressive Yield Strength 152 MPa
22000 psi
ASTM D695
Sumitomo Bakelite North America 2-530 Short-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Am..
Compressive Yield Strength 152 MPa
22000 psi
ASTM D695
Sumitomo Bakelite North America 52-20-30 Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ..
Compressive Yield Strength 151.7 MPa
22000 psi
ISO 604
Hexcel® HexPly® 916 120°C Curing Epoxy Matrix
HexPly® 916 is a self-extinguishing modified epoxy matrix system with very high self adhesive properties. It is an ideal system for single shot honeycomb sandwich manufacture, with good drape chara..
Compressive Yield Strength 151.7 MPa
22000 psi
Abatron AboCast/AboCure 8109-13
Liquid hardener version of AboCast/AboCure 8109-11.Processing: 100/23 pbw; Potlife: 3-5 h/20°C (68°F), 1-3 h/40°C (105°F), 0.5-1 h/60°C (140°F); mix at RT; cures in: 30 mins/60°C (140°F), 45..
Compressive Yield Strength 152 MPa
22000 psi
ASTM D695
Adell AT-14 Nylon 66, 20% Glass Reinforced; Impact Modified
Data provided by Adell Plastics, Inc.
Compressive Yield Strength 152 MPa
22000 psi
ASTM D695
Adell AT-34 Nylon 66, 20% Glass Reinforced; Impact Modified
Data provided by Adell Plastics, Inc.
Compressive Yield Strength 152 MPa
22000 psi
ASTM D695
Sumitomo Bakelite North America FS-4 Short-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A..
Compressive Yield Strength 152 MPa
22000 psi
ASTM D695
Sumitomo Bakelite North America RX® 1-501AN Mineral Filled Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ..
Compressive Yield Strength 152 - 189 MPa
22000 - 27400 psi
Average value: 172 MPa Grade Count:4