Material Notes:
HexPly® 916 is a self-extinguishing modified epoxy matrix system with very high self adhesive properties. It is an ideal system for single shot honeycomb sandwich manufacture, with good drape characteristics. HexPly® 916 exhibits excellent environmental resistance, and good service temperature capability.HexPly® 916 prepregs are only available in fabric form.Features: Self-extinguishing, High strength retention to 120°C, Excellent adhesion to honeycomb, Suitable for a range of cure pressure (0.8 to 10 bar), Tough matrix system, Low tack
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
Cured
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ISO R527 type 1
Elongation at Yield 1.4 %
1.4 %
ISO R527 type 1
10.3 %
10.3 %
Compression Strain; ISO 604
Tensile Modulus 4.17 GPa
605 ksi
ISO R527 type 1
Flexural Yield Strength 92.0 MPa
13300 psi
ISO 178
Flexural Modulus 3.78 GPa
548 ksi
ISO 178
Compressive Yield Strength 151.7 MPa
22000 psi
ISO 604
Shear Modulus 1.52 GPa
220 ksi
ISO R527 type 1
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 145 °C
293 °F
DMTA
Processing Properties Metric English Comments
Shelf Life >= 12.0 Month

@Temperature -18.0 °C
>= 12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Tack Life (days) 30