Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 151.7 MPa | 22000 psi | ISO 604 |
Hexcel® HexPly® 916 120°C Curing Epoxy Matrix HexPly® 916 is a self-extinguishing modified epoxy matrix system with very high self adhesive properties. It is an ideal system for single shot honeycomb sandwich manufacture, with good drape chara.. |
|||
Compressive Yield Strength | 151.7 MPa | 22000 psi | |
Abatron AboCast/AboCure 8109-13 Liquid hardener version of AboCast/AboCure 8109-11.Processing: 100/23 pbw; Potlife: 3-5 h/20°C (68°F), 1-3 h/40°C (105°F), 0.5-1 h/60°C (140°F); mix at RT; cures in: 30 mins/60°C (140°F), 45.. |