Mechanical Properties Metric English Comments
Compressive Yield Strength 131 - 172 MPa
19000 - 25000 psi
Average value: 145 MPa Grade Count:3
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
Compressive Yield Strength 152 - 172 MPa
22000 - 25000 psi
Average value: 164 MPa Grade Count:4
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Compressive Yield Strength 89.6 - 172 MPa
13000 - 25000 psi
Average value: 134 MPa Grade Count:12
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Copyright © lookpolymers.com All Rights Reserved