Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sumitomo Bakelite North America RX® 1-501AN Mineral Filled Diallyl Phthalate

Category Polymer , Thermoset , Diallyl Phthalate (DAP) , Diallyl Phthalate (DAP), Cast, Mineral Filler , Filled/Reinforced Thermoset
Manufacturer Sumitomo Bakelite North America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sumitomo Bakelite North America RX® 1-501AN Mineral Filled Diallyl Phthalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North America, Inc.
Physical Properties Metric English Comments
Density 1.73 g/cc
0.0625 lb/in³
ASTM D792
Apparent Bulk Density 0.670 g/cc
0.0242 lb/in³
Water Absorption 0.40 %
0.40 %
48 hours, 50°C. ASTM D570
Linear Mold Shrinkage 0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
Compression Molding. ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 52.0 MPa
7540 psi
ASTM D638
Flexural Yield Strength 103 MPa
14900 psi
ASTM D790
Flexural Modulus 9.00 GPa
1310 ksi
ASTM D790
Compressive Yield Strength 152 MPa
22000 psi
ASTM D695
Izod Impact, Notched 0.240 J/cm
0.450 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 34.0 µm/m-°C

@Temperature 20.0 °C
18.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 149 °C
300 °F
ASTM D648A
Oxygen Index 24 %
24 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 3.7

@Frequency 1e+6 Hz
3.7

@Frequency 1e+6 Hz
Wet
4.3

@Frequency 1000 Hz
4.3

@Frequency 1000 Hz
Wet
Dielectric Strength 15.0 kV/mm
381 kV/in
Wet, step-by-step. ASTM D149
16.0 kV/mm
406 kV/in
Wet, short term. ASTM D149
Dissipation Factor 0.015

@Frequency 1000 Hz
0.015

@Frequency 1000 Hz
Wet; ASTM D150
0.019

@Frequency 1e+6 Hz
0.019

@Frequency 1e+6 Hz
Wet; ASTM D150
Arc Resistance 135 sec
135 sec
ASTM D495
Processing Properties Metric English Comments
Processing Temperature 160 - 180 °C
320 - 356 °F
Mold temperature