KYDEX® 152WG Capped Wood Grain Thermoplastic Sheet

Category Polymer , Thermoplastic
Manufacturer KYDEX LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KYDEX® 152WG Capped Wood Grain Thermoplastic Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Super tough, durableHigh extensibility, rigidity, abrasion resistance and fire retardancyMore rigid than most thermoplastics, parts deform less when loadedOutstanding resistance to breakageSuperior scratch and abrasion resistanceSuggested Applications:Kiosk HousingsExhibits and DisplaysStore Fixture ComponentsContract Furniture ComponentsInformation provided by Kydex, LLC.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 42.0 MPa
6090 psi
ASTM D638
Flexural Strength 66.0 MPa
9570 psi
ASTM D790
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Izod Impact, Notched 7.95 J/cm
14.9 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 75.6 °C
168 °F
ASTM D648
Flammability, UL94 V-0
V-0
Descriptive Properties Value Comments
Scratch Resistance (g) > 2000
Hoffman
Surface Burning Characteristics: Flame Spread/Smoke Class 1/A
ASTM E84; 1 mm and less