Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

KYDEX® 311 MB Co-Extruded High Impact Fire-Rated Thermoplastic Sheet with Microban® Antimicrobial

Category Polymer , Thermoplastic
Manufacturer KYDEX LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KYDEX® 311 MB Co-Extruded High Impact Fire-Rated Thermoplastic Sheet with Microban® Antimicrobial.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Color-matched cap, black or off-white substrateThickness ranging from 1.5 mm to 8.9 mmToughness and durabilityEasy to form with good part definitionChemical resistantFire retardantExcellent fabrication qualitiesMicroban® antimicrobial technology inhibits the growth of bacteria that can cause stains, odors and product deterioration.Microban® technology is built-in to the sheet so it won't wash or wear away and lasts for the lifetime of the product.Microban® technology keeps the surface cleaner between cleanings.Suggested Applications:Exhibits and DisplaysStore Fixture ComponentsMedical ProductsMachine HousingsInformation provided by Kydex, LLC.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 42.0 MPa
6090 psi
ASTM D638
Flexural Strength 66.0 MPa
9570 psi
ASTM D790
Flexural Modulus 2.482 GPa
360.0 ksi
ASTM D790
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 66.7 °C
152 °F
unannealed; ASTM D648
75.5 °C
168 °F
annealed; ASTM D648
Flammability, UL94 V-0
V-0
5VA
5VA