SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP FARADEX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
1.12 g/cc
0.0405 lb/in³
ASTM D792
Moisture Absorption 0.200 %
0.200 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0018 cm/cm

@Time 86400 sec
0.0018 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0027 cm/cm

@Time 86400 sec
0.0027 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.0 MPa
5370 psi
ISO 527
39.0 MPa
5660 psi
ASTM D638
Tensile Strength, Yield 39.0 MPa
5660 psi
ISO 527
42.0 MPa
6090 psi
ASTM D638
Elongation at Break 3.3 %
3.3 %
ISO 527
8.6 %
8.6 %
ASTM D638
Elongation at Yield 2.2 %
2.2 %
ASTM D638
2.2 %
2.2 %
ISO 527
Tensile Modulus 2.50 GPa
363 ksi
1 mm/min; ISO 527
2.99 GPa
434 ksi
50 mm/min; ASTM D638
Flexural Strength 66.0 MPa
9570 psi
ISO 178
75.0 MPa
10900 psi
ASTM D790
Flexural Modulus 2.50 GPa
363 ksi
ISO 178
2.81 GPa
408 ksi
ASTM D790
Izod Impact, Notched 0.580 J/cm
1.09 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.86 J/cm
5.36 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 11.0 J
8.11 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 78.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
43.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
79.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
44.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 75.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C
196 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
97.0 °C

@Thickness 3.20 mm
207 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
87.0 °C

@Thickness 3.20 mm
189 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 100 - 1.00e+6 ohm-cm
100 - 1.00e+6 ohm-cm
ASTM D257
Surface Resistance 10 ohm - 1e+05
10 ohm - 1e+05
ASTM D257
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method