Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Plaslube® J-1/AF/15/TF/10 NAT PA66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Aramid Fiber Filled
Manufacturer Techmer ES
Trade Name Plaslube®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plaslube® J-1/AF/15/TF/10 NAT PA66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Water Absorption 0.75 %
0.75 %
24 Hrs; ASTM D570
Linear Mold Shrinkage 0.010 - 0.015 cm/cm
0.010 - 0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100 - 110
100 - 110
ASTM D785
Tensile Strength at Break 75.8 MPa
11000 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 3.52 GPa
510 ksi
ASTM D790
Izod Impact, Notched 0.454 J/cm
0.850 ft-lb/in
ASTM D256