Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 124 - 145 MPa | 18000 - 21000 psi | ASTM D790 |
Mar-Bal MB1000-15 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Flexural Strength | 124 - 145 MPa | 18000 - 21000 psi | ASTM D790 |
Mar-Bal MB3000-20NY Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Flexural Strength | 75.8 - 145 MPa | 11000 - 21000 psi | |
Bulk Molding Compounds BMC 606 Mineral Filled, Glass Reinforced Polyester Compound BMC 606 is a mineral filled, glass reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good moldability, excellent impact strength,.. |
|||
Flexural Strength | 117 - 145 MPa | 17000 - 21000 psi | |
Bulk Molding Compounds BMC T15(GP) General Purpose Molding Compound BMC T15(GP) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GP) is well suited for a variety of applications. It is av.. |