Material Notes:
Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided by Aurora Technologies.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0490 lb/in³
Water Absorption 0.40 %
0.40 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95
95
Tensile Strength, Ultimate 82.7 MPa
12000 psi
Flexural Strength 124 MPa
18000 psi
Compressive Strength 207 MPa
30000 psi
Shear Strength 68.9 MPa
10000 psi
Izod Impact, Notched 0.240 J/cm
0.450 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Mechanical
125 °C
257 °F
Electrical
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+12 ohm-cm
8.00e+12 ohm-cm
Surface Resistance 2.00e+12 ohm
2.00e+12 ohm
Dielectric Constant 4.4

@Frequency 1e+6 Hz
4.4

@Frequency 1e+6 Hz
Dielectric Strength 21.7 kV/mm
550 kV/in
Dielectric Breakdown 70000 V
70000 V
Dissipation Factor 0.037

@Frequency 1e+6 Hz
0.037

@Frequency 1e+6 Hz
Descriptive Properties Value Comments
Color Natural