Polymer Property : Tensile Stress = 10200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 70.0 MPa

@Strain 5.00 %,
Temperature 120 °C
10200 psi

@Strain 5.00 %,
Temperature 248 °F
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY
Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 70.0 MPa

@Strain 2.00 %,
Temperature 80.0 °C
10200 psi

@Strain 2.00 %,
Temperature 176 °F
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned
Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p..
Tensile Stress 70.0 MPa

@Strain 8.00 %,
Temperature 120 °C
10200 psi

@Strain 8.00 %,
Temperature 248 °F
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned
Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p..
Tensile Stress 70.0 MPa

@Strain 2.00 %,
Temperature 100 °C
10200 psi

@Strain 2.00 %,
Temperature 212 °F
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 70.0 MPa

@Strain 3.00 %,
Temperature 120 °C
10200 psi

@Strain 3.00 %,
Temperature 248 °F
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned
Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 70.0 MPa

@Strain 2.00 %,
Temperature 80.0 °C
10200 psi

@Strain 2.00 %,
Temperature 176 °F
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned
Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 70.0 MPa

@Strain 6.00 %,
Temperature 150 °C
10200 psi

@Strain 6.00 %,
Temperature 302 °F
Solvay TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY
Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The prod..
Tensile Stress 70.0 MPa

@Strain 2.00 %
10200 psi

@Strain 2.00 %
Solvay TECHNYL® A 221 PA66, DRY
Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef..
Tensile Stress 70.0 MPa

@Strain 3.00 %
10200 psi

@Strain 3.00 %
Solvay TECHNYL® A 402H1 Natural PA66, DRY
Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The ..
Tensile Stress 70.0 MPa

@Strain 4.00 %,
Temperature 100 °C
10200 psi

@Strain 4.00 %,
Temperature 212 °F
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY
Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim..
Tensile Stress 70.0 MPa

@Strain 2.00 %
10200 psi

@Strain 2.00 %
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, Conditioned
Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers..
Tensile Stress 70.0 MPa

@Strain 2.00 %,
Temperature 160 °C
10200 psi

@Strain 2.00 %,
Temperature 320 °F
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned
Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due..
Tensile Stress 70.0 MPa

@Strain 2.50 %,
Temperature 23.0 °C
10200 psi

@Strain 2.50 %,
Temperature 73.4 °F
Solvay TECHNYL® A 205F PA66, DRY
Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities..
Tensile Stress 70.2 MPa

@Strain 8.30 %,
Temperature -20.0 °C
10200 psi

@Strain 8.30 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)  (Unverified Data**)
Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri..
Tensile Stress 70.36 MPa

@Strain 1.44 %,
Temperature 40.0 °C
10200 psi

@Strain 1.44 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G15L NC010 Nylon 6  (Unverified Data**)
15% Glass Reinforced Polyamide 6Zytel 73G15L NC010 is a 15% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 70.36 MPa

@Strain 4.98 %,
Temperature 90.0 °C
10200 psi

@Strain 4.98 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610  (Unverified Data**)
20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers
Tensile Stress 70.1 MPa

@Strain 4.41 %,
Temperature 120 °C
10200 psi

@Strain 4.41 %,
Temperature 248 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66
Information provided by DuPont Performance Polymers
Tensile Stress 70.3 MPa

@Strain 4.16 %,
Temperature 90.0 °C
10200 psi

@Strain 4.16 %,
Temperature 194 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66
Information provided by DuPont Performance Polymers
Tensile Stress 70.3 MPa

@Strain 0.100 %,
Temperature 25.0 °C
10200 psi

@Strain 0.100 %,
Temperature 77.0 °F
COI Ceramics Nextel™ A-N720 Oxide Ceramic Matrix Composite, Alumina
Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air..
Tensile Stress 70.0 MPa

@Strain 1.00 %,
Temperature -40.0 °C
10200 psi

@Strain 1.00 %,
Temperature -40.0 °F
ISO 527
BASF Ultradur B 4300 G4 20% Glass Filled PBT
Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Tensile Stress 70.0 MPa

@Temperature 150 °C
10200 psi

@Temperature 302 °F
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide
Description: Ultramid® Endure is a new, glass-fiber reinforced polyamide that combines excellent heat aging resistance with the good processing properties of PA 66. Ultramid® Endure can withstand ..
Tensile Stress 70.0 MPa

@Strain 4.00 %,
Temperature 23.0 °C
10200 psi

@Strain 4.00 %,
Temperature 73.4 °F
ISO 527
BASF Ultrason S 3010 PSU
Ultrason S 3010 is an unreinforced, higher viscosity injection molding and extrusion PSU grade, tougher and with improved chemical resistance. It conforms to FDA requirements of 21 CFR 177.1655.
Tensile Stress 70.0 MPa

@Temperature 23.0 °C
10200 psi

@Temperature 73.4 °F
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone
Description: Medium viscosity injection-molding and extrusion grade with good toughness and chemical resistance (stress crack resistance), resistant against superheated steam. The property profile m..
Tensile Stress 70.0 MPa

@Time 3600 sec,
Strain 1.15 %
10200 psi

@Time 1.00 hour,
Strain 1.15 %
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. ..
Tensile Stress 70.0 MPa

@Strain 50.0 %,
Temperature 0.000 °C
10200 psi

@Strain 50.0 %,
Temperature 32.0 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66  (Unverified Data**)
Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi..