Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® 2706N Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 2706N Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Copolymer for Heavy Duty Injection Molded Applications Formolene® 2706N is a copolymer of polypropylene designed and formulated for injection molding applications. It contains a unique combination of stabilizers, nucleators and antistats, which give it an excellent balance of stiffness and impact strength. Formolene 2706N offers advantages in both processing and physical properties for applications including pails, crates and other Material Handling. Formolene® 2706N complies with the U. S. Food and Drug Administration regulation 21 CFR 177.1520(c)(3.4). This material may only be used in contact with foods of type I, II, III, IV-B, VI, VII, VIII and IX as described in Table 1 of 21 CFR 176.170(c)Specimens were injection molded according to the conditions specified in ASTM D4101Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 7.0 g/10 min

@Temperature 230 °C
7.0 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 18.6 MPa
2700 psi
2" (50mm) per min; ASTM D638
Elongation at Yield 7.0 %
7.0 %
2" (50mm) per min; ASTM D638
Flexural Modulus 0.862 GPa
125 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 1.39 J/cm

@Temperature -30.0 °C
2.60 ft-lb/in

@Temperature -22.0 °F
ASTM D256
1.60 J/cm

@Temperature -18.0 °C
3.00 ft-lb/in

@Temperature -0.400 °F
ASTM D256
7.26 J/cm

@Temperature 0.000 °C
13.6 ft-lb/in

@Temperature 32.0 °F
ASTM D256
7.47 J/cm

@Temperature 23.0 °C
14.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Users viewing this material also viewed the following: