Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Hifaxâ„¢ ETA-3081 Thermoplastic Olefin Resin

Category Polymer , Thermoplastic
Manufacturer LyondellBasell
Trade Name Hifax™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hifaxâ„¢ ETA-3081 Thermoplastic Olefin Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: medium high melt flow, medium modulus, paintable thermoplastic olefin resin, excellent balance of properties, excellent processability, good paintability and paint durability, good surface appearanceApplications: molded-in color and painted automotive bumper fascias, air deflectors, step pads and filler panels, license plate pocketsDescription: Hifax ETA-3081 medium high melt flow, paintable thermoplastic olefin resin has a vry good combinatio of physical properties, modability and paintability. An extemely verastile material, it was desgined for a wide variety of apinted and modled-in color automotive exterior components.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
Tool, Montell
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength, Yield 17.0 MPa
2470 psi
ASTM D638
Elongation at Break 550 %
550 %
ASTM D638
Flexural Modulus 0.550 GPa
79.8 ksi
Tangent at 0.05 in/min; ASTM D790A
Gardner Impact 34.0 J

@Temperature -30.0 °C
25.1 ft-lb

@Temperature -22.0 °F
ASTM D3029
Impact Test 22.0 J

@Temperature -30.0 °C
16.2 ft-lb

@Temperature -22.0 °F
Dynatup Impact, E at Max Load, Ductile; ASTM D3763
Tear Strength 100 kN/m
571 pli
ASTM D624
Thermal Properties Metric English Comments
Brittleness Temperature -55.0 °C
-67.0 °F
ASTM D746