Polymer Property : 300% Modulus = 0.00290 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00290 GPa
0.421 ksi
measured on films cast from a solution in toluene; ISO 37
Kraton® D1101 A (SBS) Liner Block Copolymer
Description: Kraton D1101 A polymer is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical forms identified as f..
300% Modulus 0.00290 GPa
0.421 ksi
measured on films cast from a solution in toluene; ISO 37
Kraton® D1101 B (SBS) Liner Block Copolymer
Description: Kraton D1101 B is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from South America in the physical form(s) identifi..
300% Modulus 0.00290 GPa
0.421 ksi
measured on films cast from a solution in toluene; ISO 37
Kraton® D1101 E (SBS) Liner Block Copolymer
Description: Kraton D1101 E polymer is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical forms identified as f..
300% Modulus 0.00290 GPa
0.421 ksi
ISO 37
Kraton® D1101 J (SBS) Liner Block Copolymer
Description: Kraton D1101 J is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Japan in the physical form(s) outlined in the follow..
300% Modulus 0.00290 GPa
0.421 ksi
ASM D 412
Kraton® D1102 B (SBS) Liner Block Copolymer
Description: Kraton D1102 B is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 29.5%. It is supplied from South America in the physical form identifie..
300% Modulus 0.00290 GPa
0.421 ksi
Measured on films cast from a solution in toluene; ISO 37
Kraton® D1102 E (SBS) Liner Block Copolymer
Description: Kraton D1102 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 28.5% mass. It is supplied from Europe in the physical form(s) identified below in..
300% Modulus 0.00290 GPa
0.421 ksi
Measured on films cast from a solution in toluene; ISO 37
Kraton® D1153 A (SBS) Liner Block Copolymer
Description: Kraton D1153 A is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in..
300% Modulus 0.00290 GPa
0.421 ksi
Measured on films cast from a solution in toluene; ISO 37
Kraton® D1153 E (SBS) Liner Block Copolymer
Description: Kraton D1153 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in..
300% Modulus 0.00290 GPa
0.421 ksi
ISO 37
Kraton® D1155 B (SBS) Liner Block Copolymer
Description: Kraton D1155 B is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 40% mass. It is supplied from South America as indicated in the grade nomenclature..
300% Modulus 0.00290 GPa
0.421 ksi
ISO 37
Kraton® D1155 J (SBS) Liner Block Copolymer
Description: Kraton D1155 J is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 40% mass. It is supplied from Japan in the physical form(s) outlined in the grade..
300% Modulus 0.00290 GPa
0.421 ksi
measured on films cast from a solution in toluene; ASTM D 412
Kraton® D1102 A (SBS) Liner Block Copolymer
Description: Kraton D1102 A is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in..
300% Modulus 0.00290 GPa
0.421 ksi
ISO 37
Kraton® D1102 J (SBS) Liner Block Copolymer
Description: Kraton D1102 J is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Japan in the physical form(s) identified below in the..
300% Modulus 0.00290 GPa
0.421 ksi
ASTM D412
Dynasol Solprene® 412 Thermoplastic Elastomer
Solprene 412 is a radial oil extended styrene butadiene block copolymer having 30% of styrene content, most of it forming a polystyrene block which gives the polymer a thermoplastic behavior. It is ..