Kraton® D1155 J (SBS) Liner Block Copolymer

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Kraton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D1155 J (SBS) Liner Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton D1155 J is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 40% mass. It is supplied from Japan in the physical form(s) outlined in the grade nomenclature: D1155 JOP - supplied as dusted dense pelletsD1155 JO - supplied as dusted crumbRegion: North America, Europe, Asia Pacific, Japan, and South America Uses: Kraton D1155 J Polymer is used as a modifier of polymers and in formulating adhesives, sealants and coatings. It is also used in compounds for technical and footwear applications.Applications: Compounding and Personal HygieneInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
Volatiles <= 0.20 %

@Temperature 110 °C,
Time 7200 sec
<= 0.20 %

@Temperature 230 °F,
Time 2.00 hour
JOP
<= 1.0 %

@Temperature 110 °C,
Time 7200 sec
<= 1.0 %

@Temperature 230 °F,
Time 2.00 hour
JO
Melt Flow 1.8 - 4.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.8 - 4.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Ash <= 0.20 %
<= 0.20 %
JOP; ISO 247
<= 1.0 %
<= 1.0 %
JO; ISO 247
Mechanical Properties Metric English Comments
Hardness, Shore A 87

@Time 30.0 sec
87

@Time 0.00833 hour
ISO 7619
Tensile Strength 28.0 MPa
4060 psi
ISO 37
Elongation at Break 800 %
800 %
ISO 37
300% Modulus 0.00290 GPa
0.421 ksi
ISO 37
Descriptive Properties Value Comments
Content Bound Styrene
40 percent