Dynasol Solprene® 412 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Dynasol
Trade Name Solprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dynasol Solprene® 412 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Solprene 412 is a radial oil extended styrene butadiene block copolymer having 30% of styrene content, most of it forming a polystyrene block which gives the polymer a thermoplastic behavior. It is oil-extended with 6 phr of Paraffinic oil. It develops properties of vulcanized rubber yet not requiring vulcanization. It is protected with a non staining antioxidant system and is essentially gel free with a very clear color. Solprene 412 is used as elastomeric modifier for asphalt and in shoe sole compounding, injection molding and other thermoplastic crafts. It is available as free flowing pellets in standard paper bags, super-sacs and Gaylord boxes.Information provided by Dynasol.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
DIN 53479
Viscosity 25.38 cP
25.38 cP
Toluene solution, 5.23%; NM 300-11
Brookfield Viscosity 18000 cP
18000 cP
0.25; ASTM D2994
Melt Index of Compound <= 0.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 0.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Collected Volatile Condensable Material <= 1.0 %
<= 1.0 %
ASTM D1416
Mechanical Properties Metric English Comments
Hardness, Shore A 79
79
Shore A2; ASTM D2240
Tensile Strength at Break 14.4 MPa
2090 psi
ASTM D412
Elongation at Break 675 %
675 %
ASTM D412
300% Modulus 0.00290 GPa
0.421 ksi
ASTM D412
Descriptive Properties Value Comments
Antioxidant Content 1.1 %
NM 300-52
Paraffinic Oil Content 4-8 phr
NM 300-54
Polystyrene Min 28 %
NM 202-27
Users viewing this material also viewed the following: