Description: Kraton D1101 B is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from South America in the physical form(s) identified:Kraton D1101 BT - supplied as a dusted porous pelletKraton D1101 BTM - supplied as a dusted powderRegion: Asia Pacific, Europe, Japan, North America and South AmericaUses: Kraton D1101 B is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatings.Applications: Bitumen Modification; Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and RoofingInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Bulk Density 0.400 g/cc
0.0145 lb/in³
ASTM D 1895 method B
Volatiles <= 0.30 %
<= 0.30 %
KM 04
Brookfield Viscosity 3000 - 5000 cP
3000 - 5000 cP
Measured on 25% mass solution in toluene at 25°C; KM 06
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ash 0.30 - 0.60 %
0.30 - 0.60 %
BT; ISO 247
<= 5.0 %
<= 5.0 %
BTM; ISO 247
Mechanical Properties Metric English Comments
Hardness, Shore A 70

@Time 10.0 sec
70

@Time 0.00278 hour
Measure on compression molded slabs; ISO 868
Tensile Strength 33.0 MPa
4790 psi
measured on films cast from a solution in toluene; ISO 37
Elongation at Break 880 %
880 %
Measured on films cast from a solution in toluene; ISO 37
300% Modulus 0.00290 GPa
0.421 ksi
measured on films cast from a solution in toluene; ISO 37
Descriptive Properties Value Comments
Content Antioxidants
>0.1%, KM 08
Polystyrene
30-32%, KM 03
Total Extractables
<1.0%, KM 05
Copyright © lookpolymers.com All Rights Reserved