Kraton® D1102 J (SBS) Liner Block Copolymer

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Kraton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D1102 J (SBS) Liner Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton D1102 J is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Japan in the physical form(s) identified below in the grade nomenclature: D1102 JS - supplied as porous pellets dusted with amorphous silicaD1102 JSZ - supplied as porous pellets dusted with amorphous silica Region: Europe, South America, Asia Pacific, Japan, and North America Uses: Kraton D1102 J is used as an ingredient in formulating adhesives, sealants and coatings. It may also find use as a modifier of bitumen and polymers. Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Roads and Roofing; Medical; Packaging and Polymod; and Personal CareInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Volatiles <= 1.0 %

@Temperature 110 °C,
Time 7200 sec
<= 1.0 %

@Temperature 230 °F,
Time 2.00 hour
Viscosity 800 - 1600 cP
800 - 1600 cP
25% Toluene Solution at 25°C; KM 06
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ash <= 1.0 %
<= 1.0 %
JS, JSZ; ISO 247
Mechanical Properties Metric English Comments
Hardness, Shore A 70

@Time 30.0 sec
70

@Time 0.00833 hour
ISO 7619
Tensile Strength 33.0 MPa
4790 psi
ISO 37
300% Modulus 0.00290 GPa
0.421 ksi
ISO 37
Descriptive Properties Value Comments
Content Polystyrene
30%, KM 03