Mechanical Properties Metric English Comments
Modulus of Elasticity 0.225 - 7.80 GPa
32.6 - 1130 ksi
Average value: 2.37 GPa Grade Count:101
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Modulus of Elasticity 1.70 - 7.80 GPa

@Temperature 60.0 - 150 °C
247 - 1130 ksi

@Temperature 140 - 302 °F
Average value: 4.22 GPa Grade Count:6
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Modulus of Elasticity 4.30 - 7.80 GPa

@Temperature 60.0 - 120 °C
624 - 1130 ksi

@Temperature 140 - 248 °F
Average value: 6.02 GPa Grade Count:2
Overview of materials for Polyphenylene Ether, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu..
Modulus of Elasticity 2.70 - 7.80 GPa

@Temperature 60.0 - 150 °C
392 - 1130 ksi

@Temperature 140 - 302 °F
Average value: 4.75 GPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..