Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 2.70 GPa | >= 392 ksi | ISO.178 DN.53452 |
Polimersan Plastics POLIPOM® (POM) POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional.. |
|||
Modulus of Elasticity | 2.70 GPa | 392 ksi | 4 mm thick;10.0 mm wide molded rod; ISO 178 |
Premix Thermoplastics PRE-ELEC® PC/ABS 1420 PRE-ELEC PC/ABS 1420 is a conductive thermoplastic compound based on a PC/ABS blend. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PR.. |
|||
Modulus of Elasticity | 2.70 GPa | 392 ksi | ISO 527-1 |
Shell Carilon® DB6F0A10 Polyketone, Flame-Retarded (V-0) Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6F0A10 is a flame-retarded injection molding grade with mechanical properties which classify it a.. |
|||
Modulus of Elasticity | >= 2.70 GPa | >= 392 ksi | ISO.178 DN.53452 |
Polimersan Plastics POLIPOM® (POM) POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional.. |
|||
Modulus of Elasticity | 2.70 - 8.56 GPa | 392 - 1240 ksi | Average value: 5.21 GPa Grade Count:19 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Modulus of Elasticity | 2.70 GPa | 392 ksi | |
Lehmann & Voss LUVOCOM® 50/TF/15/NAT Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Modulus of Elasticity | 2.70 GPa | 392 ksi | |
Lehmann & Voss LUVOCOM® 80-7353/NAT Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Modulus of Elasticity | 2.70 GPa | 392 ksi | |
Lehmann & Voss LUVOCOM® 80-7580 Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Modulus of Elasticity | 2.70 GPa | 392 ksi | |
Lehmann & Voss LUVOCOM® 80-7580/BK Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Modulus of Elasticity | 2.70 GPa | 392 ksi | ISO 527-2 |
Tisan TISESTER® Flame Retardant (V0). Heat Stabilized Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Modulus of Elasticity | 2.70 GPa | 392 ksi | ISO 527-2 |
Tisan TISLAMID® 6 UNR Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Modulus of Elasticity | 2.70 GPa | 392 ksi | MD; ExxonMobil Method |
ExxonMobil Metallyte™ 30MM680 OPP Film Product Description: A biaxially oriented polypropylene film, metalized on one side, heat sealable on the other side. Typically, all gauges are used laminated with other substrates on HFFS and VFFS .. |
|||
Modulus of Elasticity | 2.70 GPa | 392 ksi | Conditioned; ISO 178 |
Addiplast Addilene H 490 M20S Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.70 GPa | 392 ksi | ISO 178 |
Addiplast Addilene H 520 T40 Polypropylene Homopolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 2.70 GPa | 392 ksi | ISO 527 |
BASF Ultraform N 2320 003 UNC Q600 POM Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent. |
|||
Modulus of Elasticity | 2.70 GPa | 392 ksi | ISO 527 |
BASF Ultraform S 2320 003 UNC Q600 POM Ultraform S2320 003 UNC Q600 is an easy flowing and rapidly freezing injection molding POM grade. Contains a mold release agent. |
|||
Modulus of Elasticity | 2.70 GPa | 392 ksi | ISO 527-2 |
BASF Ultraform® S2320 003 PRO BK 00120 POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Modulus of Elasticity | 2.70 GPa | 392 ksi | ISO 527-2 |
BASF Ultraform® S2320 003 PRO POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Modulus of Elasticity | 2.70 GPa | 392 ksi | ISO 527-1/-2 |
BASF Ultramid® C3UG4 20% Glass Filled PA6/66 (Conditioned) Description: Halogen-free and phosphorus-free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire .. |
|||
Modulus of Elasticity | 2.70 - 7.80 GPa @Temperature 60.0 - 150 °C |
392 - 1130 ksi @Temperature 140 - 302 °F |
Average value: 4.75 GPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Modulus of Elasticity | 2.70 - 11.2 GPa @Temperature -40.0 - 150 °C |
392 - 1620 ksi @Temperature -40.0 - 302 °F |
Average value: 6.24 GPa Grade Count:4 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |