Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 392 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity >= 2.70 GPa
>= 392 ksi
ISO.178 DN.53452
Polimersan Plastics POLIPOM® (POM)
POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional..
Modulus of Elasticity 2.70 GPa
392 ksi
4 mm thick;10.0 mm wide molded rod; ISO 178
Premix Thermoplastics PRE-ELEC® PC/ABS 1420
PRE-ELEC PC/ABS 1420 is a conductive thermoplastic compound based on a PC/ABS blend. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PR..
Modulus of Elasticity 2.70 GPa
392 ksi
ISO 527-1
Shell Carilon® DB6F0A10 Polyketone, Flame-Retarded (V-0) Injection Molding Grade  (discontinued **)
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6F0A10 is a flame-retarded injection molding grade with mechanical properties which classify it a..
Modulus of Elasticity >= 2.70 GPa
>= 392 ksi
ISO.178 DN.53452
Polimersan Plastics POLIPOM® (POM)
POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional..
Modulus of Elasticity 2.70 - 8.56 GPa
392 - 1240 ksi
Average value: 5.21 GPa Grade Count:19
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl..
Modulus of Elasticity 2.70 GPa
392 ksi
Lehmann & Voss LUVOCOM® 50/TF/15/NAT Polycarbonate, with PTFE, easy flowing
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper..
Modulus of Elasticity 2.70 GPa
392 ksi
Lehmann & Voss LUVOCOM® 80-7353/NAT Polyacetal-copolymer, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Modulus of Elasticity 2.70 GPa
392 ksi
Lehmann & Voss LUVOCOM® 80-7580 Polyacetal-copolymer, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Modulus of Elasticity 2.70 GPa
392 ksi
Lehmann & Voss LUVOCOM® 80-7580/BK Polyacetal-copolymer, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Modulus of Elasticity 2.70 GPa
392 ksi
ISO 527-2
Tisan TISESTER® Flame Retardant (V0). Heat Stabilized Polybutylene Terephthalate
TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi..
Modulus of Elasticity 2.70 GPa
392 ksi
ISO 527-2
Tisan TISLAMID® 6 UNR Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Modulus of Elasticity 2.70 GPa
392 ksi
MD; ExxonMobil Method
ExxonMobil Metallyte™ 30MM680 OPP Film
Product Description: A biaxially oriented polypropylene film, metalized on one side, heat sealable on the other side. Typically, all gauges are used laminated with other substrates on HFFS and VFFS ..
Modulus of Elasticity 2.70 GPa
392 ksi
Conditioned; ISO 178
Addiplast Addilene H 490 M20S Flame Retardant Polypropylene, 20% Mineral Filled
Flame retardant, mineral filled, with halogensInformation provided by Addiplast.
Modulus of Elasticity 2.70 GPa
392 ksi
ISO 178
Addiplast Addilene H 520 T40 Polypropylene Homopolymer
Mineral reinforced, improved rigidityInformation provided by Addiplast.
Modulus of Elasticity 2.70 GPa
392 ksi
ISO 527
BASF Ultraform N 2320 003 UNC Q600 POM
Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent.
Modulus of Elasticity 2.70 GPa
392 ksi
ISO 527
BASF Ultraform S 2320 003 UNC Q600 POM
Ultraform S2320 003 UNC Q600 is an easy flowing and rapidly freezing injection molding POM grade. Contains a mold release agent.
Modulus of Elasticity 2.70 GPa
392 ksi
ISO 527-2
BASF Ultraform® S2320 003 PRO BK 00120 POM
Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF
Modulus of Elasticity 2.70 GPa
392 ksi
ISO 527-2
BASF Ultraform® S2320 003 PRO POM
Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF
Modulus of Elasticity 2.70 GPa
392 ksi
ISO 527-1/-2
BASF Ultramid® C3UG4 20% Glass Filled PA6/66 (Conditioned)
Description: Halogen-free and phosphorus-free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire ..
Modulus of Elasticity 2.70 - 7.80 GPa

@Temperature 60.0 - 150 °C
392 - 1130 ksi

@Temperature 140 - 302 °F
Average value: 4.75 GPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Modulus of Elasticity 2.70 - 11.2 GPa

@Temperature -40.0 - 150 °C
392 - 1620 ksi

@Temperature -40.0 - 302 °F
Average value: 6.24 GPa Grade Count:4
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Copyright © lookpolymers.com All Rights Reserved